As reported previously, tear film surface quality (TFSQ) should be considered in contact lens (CL) fitting. This study followed noninvasive keratograph tear film break-up time (NIKBUT) in CL wearers for 12 months to validate its clinical utility in predicting CL performance.
Fifty-five subjects (M/F=17/38) aged 26±4 years were prescribed silicone hydrogel or hydrogel CLs. The study included baseline measurements without CLs; 2 visits for CL fitting and control; follow-up after 3, 6, and 12 months of CL wear; and postwear visit without CLs. Ocular Surface Disease Index (OSDI), 8-Item Contact Lens Dry Eye Questionnaire (CLDEQ-8), first and mean NIKBUT (F/M-NIKBUT), fluorescein tear film break-up time (FBUT), and ocular surface staining were evaluated.
Post hoc analysis of each pair of visits showed differences between baseline and all CL visits for F-NIKBUT, M-NIKBUT, FBUT, and corneal staining. No difference was reported in symptoms. In addition, differences between baseline and postwear visits were noted in OSDI, M-NIKBUT, FBUT, and corneal staining, with three of the latter parameters showing a downward trend.
No changes in TFSQ and symptoms were reported over 12 months. Introducing NIKBUT as part of routine CL fitting is advised to improve CL fit and predict success.
Copyright © 2021 Contact Lens Association of Ophthalmologists.
About The Expert
Maryam Mousavi
Izabela K Garaszczuk
Danilo Andrade De Jesus
Dorota H Szczesna-Iskander
Richard A Armstrong
Kelly K Nichols
D Robert Iskander
References
PubMed